Ursprungsort
Jiangsu, China
Hauptsächlichrohstoff
Epoxid
Anwendungs-Methode
Spray coating, roller coating, brush coating
Product Name
Epoxy Cloud Iron Intermediate Paint
Proportion
About 1.80kg/L (after mixing)
Mixture ratio
Component A (paint): Component B (curing agent)=25:2(mass ratio)
Dry film thickness
About 100um
Theoretical dosage
About 220g/m2 (based on 40um dry film, excluding losses)
drying time
Surface drying ≤ 1h, actual drying ≤ 24h, completely dry for 7d
Maturity time
0.5h(23℃±2℃)
Applicable period
≤8h (23℃±2℃)